- Title: Member
- Status: Offline
- Registered: 11/05/2008
- From: Pakistan
- Posts: 1
Topic: Zinc Plating bath control ?
I currently use a solution of Zinc Cyanide with Caustic Soda for the electroplating bath. As the bath gets used the chemicals get depleted.
Is there a way that I can measure the chemicals or in other words, mantain or analyze the balance of the bath ?
- Title: Administrator
- Status: Offline
- Registered: 01/24/2008
- From: Rutherfordton, NC
- Posts: 31
Re: Zinc Plating bath control ?
Hello Asad,
I found an Analysis sheet for a cyanide zinc product manufactured by Luster-On Products. Rather than retyping it I will post it below as a pic. Hope it helps.


Attachments:
1.jpg
2.jpg
1.jpg
2.jpg
- Title: Administrator
- Status: Offline
- Registered: 01/24/2008
- From: Rutherfordton, NC
- Posts: 31
Re: Zinc Plating bath control ?
And also - if you are using this product and your supplier has not supplied this info for you, and taught you how to do the analysis - you should seriously consider changing suppliers. If this is the case - I suggest you speak with Luster-On - they would never leave a client in this position.