That was quick and I am glad to be on line at Finishing Talk. My special interests are Alkaline Cyanide free zinc and enviro friendly plating systems and we have a lot going on in India on these issues. Shall be happy to hear from you and readers .
Take care and regards
Sincerely
asif Nurie
_____________

finishingmarket.com

Re: Hello From asif Nurie. Interests: Cayanide Free Zinc and Enviro Freindly Plating Syst

Hello Asif Nurie,

Do you know anything about Techic's Tumble Plater and its enviornmental advantages?

Adrienne

Re: Hello From asif Nurie. Interests: Cayanide Free Zinc and Enviro Freindly Plating Syst

Hello Asif

What is the most promissing technology you have seen regarding "enviro friendly plating systems" recently?

Sincerely,

Adrienne

afnh4

Re: Hello From asif Nurie. Interests: Cayanide Free Zinc and Enviro Freindly Plating Syst

Hello Adrienne

Trivalent Chrome Plating. Alkaline Cyanide free Zinc Plating and Non Chromate Passivates for Zinc and aluminium see to be the ones.
Regards
asif
_________

afnh4

Re: Hello From asif Nurie. Interests: Cayanide Free Zinc and Enviro Freindly Plating Syst

TECHNIC Tumble Plater. Yes heard of it, but never seen a working model .
asif Nurie

vijaykansupada

Re: Hello From asif Nurie. Interests: Cayanide Free Zinc and Enviro Freindly Plating Syst

At SIC Technologies, we do carry Alkaline Non-Cyanide Zinc Plating propritory brightener system that can be operated at low zinc/ Caustic and Higher zinc/caustic baths. Can also be used with Pot.Hydroxide electrolyte. In afddition we also carry Trivalent Blue Bright Conversion coating. Unlike others our trivalent can be operated at 2% by volume conc. or less. Prottection is available up to 120 Hrs. (ASTM B-117). Normaly other trivalent chromate requires 5% by Vol.

vijaykansupada

Re: Hello From asif Nurie. Interests: Cayanide Free Zinc and Enviro Freindly Plating Syst

vijaykansupada wrote:

At SIC Technologies, we do carry Alkaline Non-Cyanide Zinc Plating propritory brightener system that can be operated at low zinc/ Caustic and Higher zinc/caustic baths. Can also be used with Pot.Hydroxide electrolyte. In afddition we also carry wink Trivalent Blue Bright Conversion coating. Unlike others our trivalent can be operated at 2% by volume conc. or less. Prottection is available up to 120 Hrs. (ASTM B-117). Normaly other trivalent chromate requires 5% by Vol.

Also we carry water soluble and water based Chloride zinc brightener system.
wink